ESTANE S175A TPU
Technical Data Sheet Type: Estane庐 S175A is a Shore 77A, polyester type thermoplastic polyurethane (TPU). Uses: Injection Molding, Extrusion *Test samples were annealed at 100o C and 24 hours at room temperature before testing. **These are typical values and should not be used for specifications. Injection Molding Guide These settings are to be used only as a guide. This is a typical injection molding temperature profile based on the Test Machine (conditions based on a 75 ton machine with a general purpose screw 鈥� L/D 17 鈥� 脴 35mm). The optimal run conditions for specific equipment will vary depending on the machine and mold design. Drying Conditions Physical Properties Standard No. Units Value Hardness ASTM D2240 Shore A 77 Specific Gravity ASTM D792 g/cm3 1.18 Mechanical Tensile Stress: ASTM D412 kgf/cm2 At *** elongation 35 At 300% elongation 65 Tensile Strength ASTM D412 kgf/cm2 300 Ultimate Elongation ASTM D412 % 800 Tear Resistance (Die C) ASTM D624 kgf/cm 80 Abrasion Loss ISO 4649 mm3 loss 40 Compression Set ASTM D395 At 23掳C X22hr % 15 At 70掳C X22hr % 30 Mold Shrinkage ASTM D955 m/m 0.025 Thermal Vicat Softening Temperature ASTM D1525 掳C |