路博润ESTANE R185A TPU
Technical Data Sheet Type: ESTANE? R185A is a Shore 85A, polyether type thermoplastic polyurethane (TPU). Uses: Injection Molding, Extrusion *Test samples were annealed at 100°C and 24 hours at room temperature before testing. **These are typical values and should not be used for specifications. Injection Molding Guide ? These settings are to be used only as a guide. This is a typical injection molding temperature profile based on the Test Machine (conditions based on a 75 ton machine with a general purpose screw – L/D 17 – ? 35mm). The optimal run conditions for specific equipment will vary depending on the machine and mold design. Drying Conditions Physical Properties Value (Metric) Unit Test Method Hardness 87 Shore A ASTM D2240 Specific Gravity 1.10 g/cm3 ASTM D792 Mechanical Tensile Stress: kgf/cm2 ASTM D412 at 100 % Elongation 60 at 300 % Elongation 100 Tensile Strength 320 kgf/cm2 ASTM D412 Ultimate Elongation 700 % ASTM D412 Tear Resistance (Die C) 95 kgf/cm ASTM D624 Abrasion Loss 45 mm3 loss ISO 4649 Compression Set 1 ASTM D395 At 23°C X22hr 15 % At 70°C X22hr 45 % Mold Shrinkage 0.015 m/m ASTM D955 Thermal Vicat Softening Temperature 90 °C ASTM D15 |